Polymer Property : Impact Test = 12.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 12.0 J

@Temperature -40.0 °C
8.85 ft-lb

@Temperature -40.0 °F
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Peak Energy; ASTM-D3763
Ineos ABS Lustran® 256 Extrusion Blending Grade
Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi..
Impact Test 12.0 J

@Temperature -30.0 °C
8.85 ft-lb

@Temperature -22.0 °F
ASTM D3763
Diamond Polymers Centrex® 825 Sheet Extrusion Grade
Centrex 825 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it ..
Impact Test 12.0 J

@Thickness 4.00 mm
8.85 ft-lb

@Thickness 0.157 in
Multi-axial, at max. force; ISO 6603-2
Azdel Plus C200B01N 20% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C200B01 is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a v..
Impact Test 12.0 J

@Temperature 23.0 °C
8.85 ft-lb

@Temperature 73.4 °F
Multi-axial, at failure, measured on flat plaques; ASTM D3763
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness)
AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Impact Test 12.0 J

@Temperature 100 °C
8.85 ft-lb

@Temperature 212 °F
Charpy-V specimens, transverse direction.
Assab Steels HOTVAR Hot Work Steel
HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue..
Impact Test 12.0 J

@Thickness 4.00 mm
8.85 ft-lb

@Thickness 0.157 in
Multi-axial, at max. load; ASTM D3763
Azdel Plus C220-B01 22% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C220-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope..
Impact Test 12.0 J

@Thickness 4.00 mm
8.85 ft-lb

@Thickness 0.157 in
Multi-axial, at max. force; ISO 6603-2
Azdel Plus C220B02N 22% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C220B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Impact Test 12.0 J

@Temperature 23.0 °C
8.85 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Verton RV006ESV_GY7E071 PA 66
Preliminary Data for 30% long glass fiber, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region.