Polymer Property : Impact Test = 130 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 130 J

@Diameter 25.4 mm,
Temperature 200 °C
95.9 ft-lb

@Diameter 1.00 in,
Temperature 392 °F
310 HB
Assab Steels 718HH Plastic Mold Material
IMPAX SUPREME is a premium-quality vacuum-degassed Cr-Ni-Mo-alloyed steel which is supplied in the hardened and tempered condition. IMPAX SUPREME is manufactured to consistently high quality standar..