Impact Test 220 J

@Thickness 6.35 mm,
Temperature -40.0 °C
162 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
rotomolded; ARM Method
NOVA Chemicals Novapol® TR-0338-UI Hexene MDPE Rotational Molding Resin
Excellent low temperature impact properties, Excellent ESCR, Good stiffness, Wide processing windowApplications: General purpose custom molding, Chemical containers, IBCs, Fish boxes, Septic tanks, ..
Impact Test 220 J

@Thickness 6.35 mm,
Temperature -40.0 °C
162 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
rotomolded; ARM Method
NOVA Chemicals Novapol® TR-0338-UIG Hexene MDPE Rotational Molding Resin
Excellent low temperature impact properties, Excellent ESCR, Good stiffness, Wide processing windowApplications: General purpose custom molding, Chemical containers, IBCs, Fish boxes, Septic tanks, ..