Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 17.6 J @Temperature 23.0 °C |
13.0 ft-lb @Temperature 73.4 °F |
Multi-Axial, Ductile; ASTM D3763 |
Flint Hills P9M6K-041A Specialty Impact Copolymer Polypropylene Features: Good clarity and impact resistance. Product does not contain animal derived components.Applications: Injection molding - durable goodsInformation provided by Flint Hills Resources. |
|||
Impact Test | 17.6 J @Temperature 23.0 °C |
13.0 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil OPTEMA™ TC 120 Molding Ethylene Methyl Acrylate Product Description: Optema TC 120 is an ethylene methyl acrylate copolymer, which can be used as an impact modifier or compatibilizer in polymer compounds. TC 120 has been processed on typical LDPE.. |
|||
Impact Test | 17.6 J @Temperature 23.0 °C |
13.0 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 728.61 Molding, extrusion and compounding resin Escorene Ultra LD 728.61 is a high vinyl acetate copolymer with low melting temperature and excellent strength properties and toughness.Availability: Latin America, North America and South America A.. |