Impact Test 258 J

@Thickness 6.35 mm,
Temperature -40.0 °C
190 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LL 8460.29 Rotational Molding Resin
Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o..
Impact Test 258 J

@Thickness 6.35 mm,
Temperature -40.0 °C
190 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LLDPE LL 8460.29 Linear Low Density Polyethylene Resin
Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o..
Impact Test 258 J

@Thickness 6.35 mm,
Temperature -40.0 °C
190 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LLDPE LLP 8460.29 Linear Low Density Polyethylene Resin
Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o..
Impact Test 258 J

@Thickness 6.35 mm,
Temperature -40.0 °C
190 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LLP8460.29 Rotational Molding Resin
Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o..
Impact Test 258 J

@Thickness 6.35 mm,
Temperature -40.0 °C
190 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
ExxonMobil LL 8460 Rotational Molding Resin  (discontinued **)
LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require optimum balance of stiffness, processabili..