Mechanical Properties Metric English Comments
Impact Test 28.0 J

@Thickness 4.00 mm
20.7 ft-lb

@Thickness 0.157 in
Multi-axial, total energy; ISO 6603-2
Azdel Plus C200B01N 20% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C200B01 is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a v..
Impact Test 28.0 J

@Thickness 4.00 mm
20.7 ft-lb

@Thickness 0.157 in
Multi-axial, at failure; ASTM D3763
Azdel Plus R300-B01 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R300-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr..
Impact Test 28.0 J

@Thickness 4.00 mm
20.7 ft-lb

@Thickness 0.157 in
Multi-axial, at failure; ASTM D3763
Azdel Plus C220-B01 22% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C220-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope..
Impact Test 28.0 J

@Thickness 4.00 mm
20.7 ft-lb

@Thickness 0.157 in
Multi-axial, total energy; ISO 6603-2
Azdel Plus C220B02N 22% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C220B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Impact Test 28.0 J

@Thickness 4.00 mm
20.7 ft-lb

@Thickness 0.157 in
Multi-axial, at failure; ASTM D3763
Azdel Plus R401-B01 40% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R401-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr..
Copyright © lookpolymers.com All Rights Reserved