Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 32.5 J @Temperature -40.0 °C |
24.0 ft-lb @Temperature -40.0 °F |
Instrumented Impact, Total Energy; ASTM D3763 |