Impact Test 41.0 J

@Temperature -18.0 °C
30.2 ft-lb

@Temperature -0.400 °F
ASTM D3763
Diamond Polymers Centrex® 601 Profile Extrusion Grade AES
Centrex 601 resin is a very high-impact, low-gloss AES (acrylonitrile-ethylene-propylene-styrene) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can..