Mechanical Properties Metric English Comments
Impact Test 6.00 J

@Temperature -30.0 °C
4.43 ft-lb

@Temperature -22.0 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl GTX GTX8430W PPE+PA
30% Glass Reinforced PPE+PA Alloy. Typically used for automotive connectors.This data was supplied by SABIC-IP for the Americas region.
Impact Test 6.00 J

@Temperature -40.0 °C
4.43 ft-lb

@Temperature -40.0 °F
ASTM D3763
Diamond Polymers Centrex® 485 Sheet Extrusion Grade
Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it..
Impact Test 6.00 J

@Temperature 23.0 °C
4.43 ft-lb

@Temperature 73.4 °F
Multi-axial, at failure, measured on flat plaques; ASTM D3763
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness)
AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..