Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 58.0 J @Temperature -30.0 °C |
42.8 ft-lb @Temperature -22.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® MC9000 PC+ABS AUTOMOTIVE. PC+ABS; high heat resistant. Ductile at room temperature. Excellent flow.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 58.0 J @Temperature -30.0 °C |
42.8 ft-lb @Temperature -22.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® MC9000 PC+ABS (Asia Pacific) AUTOMOTIVE. PC+ABS; high heat resistant. Ductile at room temperature. Excellent flow.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 58.0 J @Thickness 4.00 mm |
42.8 ft-lb @Thickness 0.157 in |
Multi-axial, at failure; ASTM D3763 |
Azdel Plus U421-B01 42% Directionalized Continuous Fiber Mat / PP Resin Matrix AZDEL® U421-B01 is a glass mat thermoplastic laminate based upon a combination of random oriented continuous fiber mat and oriented fiber mat contained within a polypropylene resin matrix. This co.. |
|||
Impact Test | 58.0 J @Thickness 4.00 mm |
42.8 ft-lb @Thickness 0.157 in |
Multi-axial, at max. force; ISO 6603-2 |
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This.. |