Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 7.90 J @Temperature 23.0 °C |
5.83 ft-lb @Temperature 73.4 °F |
Multi-axial, at max. load; ASTM D3763 |
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (6 mm Molded Thickness) AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Impact Test | 7.90 J @Temperature 23.0 °C |
5.83 ft-lb @Temperature 73.4 °F |
Multi-axial, at failure, measured on flat plaques; ASTM D3763 |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |