Mechanical Properties Metric English Comments
Impact Test 6.22 J

@Temperature -30.0 °C
4.59 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
Styron Pulse® 759 ABS + Polycarbonate, 15% Glass Reinforced
PULSE® 759 Engineering resin is a 15% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 759 Engineering resin has been used..