Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 8.50 J @Temperature -30.0 °C |
6.27 ft-lb @Temperature -22.0 °F |
Multi-Axial Impact, Fractovis J; Energy Max; ASTM-D3763 |
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |
|||
Impact Test | 8.50 J @Temperature 23.0 °C |
6.27 ft-lb @Temperature 73.4 °F |
Multi-axial, at failure, measured on flat plaques; ASTM D3763 |
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (5 mm Molded Thickness) AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |