Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 64.0 J @Temperature 23.0 °C |
47.2 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Lexan® EXRL0662 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |