Polymer Property : Impact Test = 78.6 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 78.6 J

@Thickness 3.17 mm,
Temperature -40.0 °C
58.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
ExxonMobil HDPE HD 8760.29 High Density Polyethylene Resin
Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal..
Impact Test 78.6 J

@Thickness 3.17 mm,
Temperature -40.0 °C
58.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
ExxonMobil HDPE HD P8760.29 High Density Polyethylene Resin
Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal..
Impact Test 78.6 J

@Thickness 3.17 mm,
Temperature -40.0 °C
58.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
ExxonMobil HDP8760.29 Rotational Molding Resin
Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal..
Impact Test 78.6 J

@Thickness 3.17 mm,
Temperature -40.0 °C
58.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
ExxonMobil HD 8760.29 Rotational Molding Resin
Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal..