Mechanical Properties Metric English Comments
Impact Test 11.3 J

@Temperature 23.0 °C
8.33 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Pulse® 759 ABS + Polycarbonate, 15% Glass Reinforced
PULSE® 759 Engineering resin is a 15% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 759 Engineering resin has been used..