Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 110 J @Thickness 6.34 mm, Temperature -40.0 °C |
81.1 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM |
Braskem RD34U3 LLDPE Rotomolding Polyethylene The resin RD34U3 is a linear low-density polyethylene, 1-butene based, with excellent processability and a good balance of stiffness and impact strength. It contains long term UV6 stabilization and .. |