Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 94.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
70.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM |
ExxonMobil LL 8460.29 Rotational Molding Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Impact Test | 94.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
70.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM |
ExxonMobil LLDPE LL 8460.29 Linear Low Density Polyethylene Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Impact Test | 94.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
70.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM |
ExxonMobil LLDPE LLP 8460.29 Linear Low Density Polyethylene Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Impact Test | 94.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
70.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM |
ExxonMobil LLP8460.29 Rotational Molding Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Impact Test | 94.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
70.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM |
ExxonMobil LL 8460 Rotational Molding Resin
(discontinued **) LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require optimum balance of stiffness, processabili.. |