Polymer Property : PENT = 3000 hour Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
PENT >= 3000 hour
>= 3000 hour
ASTM F 1473
Total XT10 N Natural HDPE, pipe
Applications: Potable water, industrial and mining, sewer and sewer relining, gas and oil gathering, general pipe relining, pipe coatingInformation provided provided by Total Petrochemicals.Total Pe..