Polymer Property : Hydrostatic Design Basis = 36.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hydrostatic Design Basis 36.5 MPa
5300 psi
Hydrostatic Crush Strength (12,000 feet)
Engineered Syntactic Systems SF-38 Subsea Syntactic Void Filler
SF-38 is a specially engineered syntactic formulated to serve as a void filler for subsea applications. The material is provided as a three-part kit that is mixed and poured into any free-flood cavi..