Polymer Property : 100% Modulus = 0.000179 GPa
Polymer Property :
100% Modulus =
0.000179 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
100% Modulus
0.000179
GPa
0.0260
ksi
Shin-Etsu Silicones LIMSâ„¢ KE2004-10A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.