Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00101 GPa | 0.146 ksi | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-40A/B Elastomer KE-1950-40 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |