Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 0.00159 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00159 GPa
0.230 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 20.0 PHR Wacker HDK N20 Filler
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
100% Modulus 0.00159 GPa
0.230 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 20.0 PHR Wacker HDK N20 Filler
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
100% Modulus 0.00159 GPa
0.230 ksi
ASTM D 412
CPT C-Flex® R70-082 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
100% Modulus 0.00159 GPa
0.230 ksi
ASTM D638
Colorite Polymers 4543 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Copyright © lookpolymers.com All Rights Reserved