Polymer Property : 100% Modulus = 0.00168 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00168 GPa
0.244 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Non-Black Peroxide Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00168 GPa
0.244 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Non-Black Peroxide Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00168 GPa
0.244 ksi
ISO 37
PolyOne Elastamax XL 1092-35 TPU-Based Thermoplastic Elastomer  (discontinued **)
This is a general purpose thermoplastic elastomer based on modified TPU technology. Physical Form: Pellet. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hanna and Geon merged..