Polymer Property : 100% Modulus = 0.00173 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00173 GPa
0.251 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® 2850PE Thermoplastic Elastomer
Elastocon® 2850PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2850PE is FDA compliant and well suited for..