Mechanical Properties Metric English Comments
100% Modulus 0.00372 GPa
0.540 ksi
Spartech E65650 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
100% Modulus 0.00372 GPa
0.539 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.5 PHR Sulfur
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man..
100% Modulus 0.00372 GPa
0.540 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FT 2350 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FT 2350 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..
100% Modulus 0.00372 GPa
0.539 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.5 PHR Sulfur
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man..