Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00386 GPa | 0.560 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 1060 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00386 GPa | 0.560 ksi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 1060 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00386 GPa | 0.560 ksi | ASTM D412; ISO 37; DIN 53504 |
Advanced Polymer Alloys DURACRYN 8070 NC Thermoplastic Rubber Information provided by Advanced Polymer Alloys |