Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00434 GPa | 0.629 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-680A Solid Polyurethane Elastomer MDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
100% Modulus | 0.00434 GPa | 0.630 ksi | ASTM D412 |
SK Chemicals SKYTHANE® S385A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.00434 GPa | 0.630 ksi | ASTM D638 |
Colorite Polymers 6533 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00434 GPa | 0.630 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FC 2261Q Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2261Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
100% Modulus | 0.00434 GPa | 0.630 ksi | ASTM D638 |
Colorite Polymers 6577 Non-Phthalate 77 Series Vinyl Compound Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio.. |