Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00439 GPa | 0.636 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 2890 Thermoplastic Elastomer Elastocon® 2890 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2890 is FDA compliant and well suited for cons.. |
|||
100% Modulus | 0.00439 GPa | 0.637 ksi | Press Cure 10 Minutes @ 350°C |
3M Dyneon™ RA 5300 High Performance Rubber Additive 3M™ Dynamar™ RA 5300 High Performance Rubber Additive is designed for use at low loadings to improve the processing in extrusion and molding operations. It utilizes unique chemistry which makes it.. |