100% Modulus 0.00450 GPa
0.653 ksi
ISO/R527
Polykemi AB POLYelast TPE Z900 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
100% Modulus 0.00450 GPa
0.653 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3480N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
100% Modulus 0.00450 GPa
0.653 ksi
Lubrizol Estane® ZHF 78AT0 Thermoplastic Polyurethane, Flame Retardant
Type: Estane® ZHF 78AT0 NAT021 is a soft, polyether based, NHFR thermoplastic polyurethane (TPU) compound.Features: Soft, transparent, flame retardant.Uses: Wire and CableAvailable in Europe, Middl..
100% Modulus 0.00450 GPa
0.653 ksi
ASTM D412
UBE UBEPOL VCR412 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel..
100% Modulus 0.00450 GPa
0.653 ksi
ASTM D412
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane
Features: Highly Elastic Compound and Good Recovery for a Rubber-Like CharacterUses: Flat Die/Film Extrusion and Blown Film and Injection Molding and Profile ExtrusionAvailable in Americas, Europe, ..
100% Modulus 0.00450 GPa
0.653 ksi
ASTM D412
Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane
Features: High moisture vapor transmission. Good low temperature properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and ..
100% Modulus 0.00450 GPa
0.653 ksi
ASTM D412
Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane
Features: Transparent flame retardant compoundUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
100% Modulus 0.00450 GPa
0.653 ksi
DIN 53504
Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00450 GPa
0.653 ksi
ISO 37
Lubrizol ESTANE® GP80AE Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00450 GPa
0.653 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4725P Medium Hardness Dense Extrusion
FormulationNordel® IP 4725P
100% Modulus 0.00450 GPa
0.653 ksi
Press cure 15 minutes@ 180°C
3M Dyneon™ FPO 3741 Fluoroelastomer
Information provided by the Dyneon division of 3M.
100% Modulus 0.00450 GPa
0.653 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer
A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj..
100% Modulus 0.00450 GPa
0.653 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer
A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex..