Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 0.00945 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00945 GPa
1.37 ksi
-30% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering Perlast® G70R Red Perfluoroelastomer
Excellent chemical resistance, steam resistance and good mechanical properties. Color coded for identification.Applications: Specially developed for critical applications where good chemical resista..