Mechanical Properties Metric English Comments
100% Modulus 0.009804 GPa
1.422 ksi
ASTM D638
SK Chemicals SKYTHANE® U1731C Magnetic Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
100% Modulus 0.009804 GPa
1.422 ksi
ASTM D638
SK Chemicals SKYTHANE® UB220 Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta..