Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 0.0136 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.0136 GPa
1.97 ksi
ASTM D412
Precision Polymer Engineering Perlast® G70K Perfluoroelastomer
Special white compound with wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Recommended f..
100% Modulus 0.0136 GPa
1.97 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3145D Thermoplastic Elastomer
A high hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3145D can be processed by injection blow molding, molding or ..
100% Modulus 0.0136 GPa
1.97 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3445D Thermoplastic Elastomer
A NSF certified, high hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inje..
100% Modulus 0.0136 GPa
1.97 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3445DN Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
100% Modulus 0.0136 GPa
1.97 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® SMR1555 Thermoplastic Polyolefin Elastomer
Elastocon® SMR1555 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E..