Mechanical Properties Metric English Comments
100% Modulus 0.0143 GPa
2.07 ksi
JIS-A-5756
Denka VINYKON M2510 PVC, M grade for soft injection molding
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..