Polymer Property : 100% Modulus = 0.0178 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.0178 GPa
2.58 ksi
ASTM D412-80
DuPont Performance Polymers Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Peroxide Cured Carbon Black Filled Compound
Carbon black compound with 100 parts Hypalon; 40 parts carbon black; 20 parts magnesia; and 5.8 parts Varox® DBPH-50. Physical property data below (except mooney viscosity) are for vulcanizate. Ma..