Polymer Property : 100% Modulus = 0.0260 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.0260 GPa
3.77 ksi
ISO 37
Lubrizol ESTANE® GP72DB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 72DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, TranslucentAvailable in EuropeInformati..
100% Modulus 0.0260 GPa
3.77 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1164 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.