Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00124 GPa | 0.180 ksi | ASTM D412 |
Huntsman IROGRAN® PS 455-215 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
100% Modulus | 0.00124 GPa | 0.180 ksi | |
Mearthane Durethaneâ„¢ F DF-640A Closed Cell Foam Polyurethane MDI backbone: ester.Shore 00 Hardness: 85Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient.. |
|||
100% Modulus | 0.00124 GPa | 0.180 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys DuraGrip™ DGR 6040 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6040 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6040 NC/BK have
an excellent soft t.. |
|||
100% Modulus | 0.00124 GPa | 0.180 ksi | |
3M 8440 Silicone Rubber Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators 8440 Series are open ended, silicone rubber, tubular sleeves. The sleeves are factory expanded and assembled on a removable supporting plastic core. Each rubber.. |
|||
100% Modulus | 0.00124 GPa | 0.180 ksi | ASTM D412 |
Advanced Polymer Alloys DuraGrip™ 6840 Thermoplastic Elastomer With its true rubber look and feel, DuraGrip® TPE improves the performance and appearance of virtually any consumer or light industrial product. Its one of the most versatile materials in APAs exte.. |
|||
100% Modulus | 0.00124 GPa | 0.180 ksi | cured 15 mins @ 150°C |
ACC QSil 553 QSI Quantum Silicones Silicone Potting Material QSil 553 is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a flame retardant, thermally conductive, low modulus material that is readi.. |