Mechanical Properties Metric English Comments
100% Modulus 0.00145 GPa
0.210 ksi
heat aged one week at 300ºF
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00145 GPa
0.210 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 15.0 PHR Wacker HDK N20 Filler
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
100% Modulus 0.00145 GPa
0.210 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N990 (MT) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00145 GPa
0.210 ksi
ASTM D412
Huntsman IROGRAN® PS 370-202 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
100% Modulus 0.00145 GPa
0.210 ksi
heat aged one week at 300ºF
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00145 GPa
0.210 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 15.0 PHR Wacker HDK N20 Filler
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
100% Modulus 0.00145 GPa
0.210 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N990 (MT) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..