Polymer Property : 100% Modulus = 0.235 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00162 GPa
0.235 ksi
Injection molded plaques, Die C, Cross Direction; ASTM D412
Kraton® G2705 GU (SEBS) Compound
Description: Kraton G2705 GU-N is an easy processing material designed for applications where FDA regulations are required. The material exhibits high resilience, low compression set, and good punct..
100% Modulus 0.00162 GPa
0.235 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 30.0 PHR Wacker HDK N20 Filler
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
100% Modulus 0.00162 GPa
0.235 ksi
ASTM D638
Colorite Polymers 3511-02 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00162 GPa
0.235 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 30.0 PHR Wacker HDK N20 Filler
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..