Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00197 GPa | 0.285 ksi | ASTM D412 |
Huntsman IROGRAN® PS 456-202 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |