Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00230 GPa | 0.333 ksi | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-60A/B Elastomer KE-1950-60 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
100% Modulus | 0.00230 GPa | 0.333 ksi | ASTM D412 |
Advanced Polymer Alloys Alcryn® 2160 BK Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |