100% Modulus 0.00246 GPa
0.357 ksi
Shin-Etsu Silicones LIMSâ„¢ KEG2000-60A/B Elastomer
KEG2000-60 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum..