Mechanical Properties Metric English Comments
100% Modulus 0.00345 GPa
0.500 ksi
ASTM D412
Precision Polymer Engineering Perlast® G67P Translucent Perfluoroelastomer
A translucent beige compound with semi-crystalline perfluoropolymer nano-filler, specially developed to meet the demands of the semiconductor and bio-analytical industries. Compatible with fluorine ..
100% Modulus 0.00345 GPa
0.500 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 305ºF Cure Temperature
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00345 GPa
0.500 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00345 GPa
0.500 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00345 GPa
0.500 ksi
ASTM D412
Huntsman KRYSTALFLEX® PE 900 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
100% Modulus 0.00345 GPa
0.500 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 305ºF Cure Temperature
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00345 GPa
0.500 ksi
ASTM D412
Lubrizol Estane® AG 8451 Thermoplastic Polyurethane
Type: Estane® AG 8451 is a polyether based aliphatic (TPU) specifically formulated to be used as an adhesive interlayer film. AG-8451 is an excellent general purpose polymer for all optical allpha..
100% Modulus 0.00345 GPa
0.500 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00345 GPa
0.500 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00345 GPa
0.500 ksi
ASTM D638
Colorite Polymers 5500 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00345 GPa
0.500 ksi
ASTM D638
Colorite Polymers 6283MG General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00345 GPa
0.500 ksi
ASTM D-638
Axiall 8651 Moldings & Extrusions Flexible PVC
A quality, low gravity extrusion compound with excellent low temperature properties. Designed for use in weatherstrips, flexible gaskets and extruded shapes.Information provided by Georgia GulfGeor..
100% Modulus 0.00345 GPa
0.500 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00345 GPa
0.500 ksi
ASTM D638
Colorite Polymers 5502-UV General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00345 GPa
0.500 ksi
Colorite Polymers 5511 Clear Extrusion Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre..
100% Modulus 0.00345 GPa
0.500 ksi
Colorite Polymers 5512 Clear Injection Molding Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c..
100% Modulus 0.00345 GPa
0.500 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..