Mechanical Properties Metric English Comments
100% Modulus 0.00440 GPa
0.638 ksi
Injection molded parts; DIN 53504
Huntsman IROGRAN® A 78 E 4506 TPU-Polyester
Introduction: IROGRAN A 78 E 4506 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop..
100% Modulus 0.00440 GPa
0.638 ksi
Taiwan PU Corporation TPU-BTB85 Breathable Grade, Blow Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), Breathable Grade, Polyether Base, Blow MoldingInformation provided by Taiwan PU Corporation.
100% Modulus 0.00440 GPa
0.638 ksi
Taiwan PU Corporation TPUI-L70 Low Temperature Resistance, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
100% Modulus 0.00440 GPa
0.638 ksi
ASTM D412
UBE UBEPOL VCR412 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel..
100% Modulus 0.00440 GPa
0.638 ksi
ISO 37
Lubrizol ESTANE® 58280 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00440 GPa

@Temperature 23.0 °C
0.638 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Florida
Lubrizol Estane® 58610 Thermoplastic Polyurethane
Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee..
100% Modulus 0.00440 GPa
0.638 ksi
DIN 53504
Lubrizol ESTANE® 58561 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00440 GPa
0.638 ksi
ISO 37
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Extrusion, Black
Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and..
100% Modulus 0.00440 GPa
0.638 ksi
ISO 37
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Extrusion, Natural
Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and..
100% Modulus 0.00440 GPa
0.638 ksi
ISO 37
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Injection Molding, Black
Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu..
100% Modulus 0.00440 GPa
0.638 ksi
ISO 37
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Injection Molding, Natural
Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu..
100% Modulus 0.00440 GPa
0.638 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4570 Dense Extruded Profile
FormulationNordel® IP 4570
100% Modulus 0.00440 GPa
0.638 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 5565 Dense Extruded Profile
FormulationNordel® IP 5565
100% Modulus 0.00440 GPa
0.638 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR7560 PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
100% Modulus 0.00440 GPa
0.638 ksi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
DuPont Performance Polymers VTR 8655 (GBL-S) , VTR 8650 8655/8650 Blend  (discontinued **)