Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00685 GPa | 0.994 ksi | |
Taiwan Sheen Soon Sheenthane® A8530 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00685 GPa | 0.994 ksi | |
Taiwan Sheen Soon Sheenthane® A8670A Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmWaterproof & breathable gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00685 GPa | 0.994 ksi | |
Taiwan Sheen Soon Sheenthane® A8820N Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00685 GPa | 0.994 ksi | |
Taiwan Sheen Soon Sheenthane® A8900F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00685 GPa | 0.994 ksi | |
Taiwan Sheen Soon Sheenthane® A8910K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00685 GPa | 0.994 ksi | |
Taiwan Sheen Soon Sheenthane® A8915K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00685 GPa | 0.994 ksi | |
Taiwan Sheen Soon Sheenthane® A8960N Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00685 GPa | 0.994 ksi | |
Taiwan Sheen Soon Sheenthane® A8970A Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmWaterproof & breathable gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00685 GPa | 0.994 ksi | |
Taiwan Sheen Soon Sheenthane® A9200B Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionHalogen-free fire-retardant gradeInformation provided by Taiwan Sheen Soon Co., LTD. |