Mechanical Properties Metric English Comments
100% Modulus 0.00700 GPa
1.02 ksi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Santoprene® 281-87 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be ..
100% Modulus 0.00700 GPa
1.02 ksi
DIN 53504
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether
Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS..
100% Modulus 0.00706 GPa
1.02 ksi
LG Chemical LGflex EBNW Plasticizer
Features: Excellent Adhesion, Transparency, and Non-endocrine disrupterApplication: PVC Food Package WrapInformation provided by LG Chemical
100% Modulus 0.00700 GPa
1.02 ksi
ISO 37
Huntsman AVALON® 90 AE Thermoplastic Polyurethane
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce..
100% Modulus 0.00700 GPa
1.02 ksi
ISO 37
Huntsman AVALON® 90 AHT DP Thermoplastic Polyurethane
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce..
100% Modulus 0.00700 GPa
1.02 ksi
Injection molded parts; DIN 53504
Huntsman IROGRAN® A 87 P 4946 TPU-Polyester
Introduction: IROGRAN A 87 P 4946 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 87 P 4946 is part of the HUNTSMAN technical ext..
100% Modulus 0.00700 GPa
1.02 ksi
Injection molded parts; DIN 53504
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester
Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi..
100% Modulus 0.00700 GPa
1.02 ksi
Press-cured 5 minutes at 190°C
DuPont Vamac® DP DIAK No. 7 Coagent Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
100% Modulus 0.00700 GPa
1.02 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1490IV Polyester Based TPU
Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd.
100% Modulus 0.00700 GPa
1.02 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-8185 Polyether-Based TPU
Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
100% Modulus 0.00700 GPa
1.02 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-8285 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
100% Modulus 0.00700 GPa
1.02 ksi
ASTM D412
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUses: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
100% Modulus 0.00700 GPa
1.02 ksi
ISO 37
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00700 GPa
1.02 ksi
ASTM D412
Lubrizol ESTANE® 58284 Ether Based Thermoplastic Polyurethane
Features: Matte finish, superior durabilityUses: Extrusion – wire and cable, General applicationAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
100% Modulus 0.00700 GPa
1.02 ksi
Cured 10 minutes at 180°C
DuPont Vamac® DP 5.5 phr Peroxide Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
100% Modulus 0.00700 GPa
1.02 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1685AB Polyester Based TPU
Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd.
100% Modulus 0.00700 GPa
1.02 ksi
DIN 53504
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer unmatched toughness and d..
100% Modulus 0.00700 GPa
1.02 ksi
ASTM D638
ELASTO UK Dryflex® 420351S SBS Based Material, 35D Hardness, Natural
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
100% Modulus 0.00700 GPa
1.02 ksi
ASTM D638
ELASTO UK Dryflex® 422351S SBS Based Material, 35D Hardness, Black
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
100% Modulus 0.00700 GPa
1.02 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1690AB Polyester Based TPU
Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd.
100% Modulus 0.00700 GPa
1.02 ksi
DIN 53504
Lubrizol ESTANE® T5191 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00703 GPa
1.02 ksi
DuPont Performance Polymers Kalrez® 6230 FFKM Perfluoroelastomer