Mechanical Properties Metric English Comments
100% Modulus 0.00710 GPa
1.03 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3190 Thermoplastic Elastomer
A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3190 can be processed by blow molding, injection molding or..
100% Modulus 0.00710 GPa
1.03 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3490N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
100% Modulus 0.00710 GPa
1.03 ksi
ISO 37
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00710 GPa
1.03 ksi
Colorite Polymers Self Frosting™ 7511SF Vinyl Compound
Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi..
100% Modulus 0.00710 GPa
1.03 ksi
Colorite Polymers 7511 Clear Extrusion Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre..
100% Modulus 0.00710 GPa
1.03 ksi
Colorite Polymers 7512 Clear Injection Molding Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c..
100% Modulus 0.00710 GPa
1.03 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FE 5623 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FE 5623 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..
100% Modulus 0.00710 GPa
1.03 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FG 5690Q Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FG 5690Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu..
100% Modulus 0.00710 GPa
1.03 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3490 Thermoplastic Elastomer
A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj..
100% Modulus 0.00710 GPa
1.03 ksi
Cured 7 min at 177°C and Post Cured 16 hr at 232°C
DuPont Performance Polymers VTR 8525 (GBLT-S) GFLT-600 Formulation  (discontinued **)
FormulationViton® GFLT 600