Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.008101 GPa | 1.175 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.008101 GPa | 1.175 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.008101 GPa | 1.175 ksi | ASTM D638 |
Colorite Polymers 8090C General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.008101 GPa | 1.175 ksi | ASTM D-638 |
Axiall 8780 Moldings & Extrusions Flexible PVC Low gravity, general purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |