Polymer Property : 100% Modulus = 1.187 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.008184 GPa
1.187 ksi
-12% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering Perlast® G70H Perfluoroelastomer
Special, pure white compound with high temperature properties and wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing p..