Polymer Property : 100% Modulus = 1.85 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 95A
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
100% Modulus 0.0128 GPa
1.85 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 95A
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
100% Modulus 0.0128 GPa
1.85 ksi
ASTM D-638
Axiall 11890 Wire & Cable Flexible PVC
High gloss, flame retardant jacketing compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0128 GPa
1.85 ksi
ASTM D-638
Axiall 14880 Wire & Cable Flexible PVC
14880 is a non-lead stabilized, 80°C rated jacket with UL recognition for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 20..
100% Modulus 0.0128 GPa
1.85 ksi
ASTM D-638
Axiall 19930 Wire & Cable Flexible PVC
THHN-THWN circuit sizes. Best suited for 105°C; 1/64 (18 AWG and larger). Rated VW-1. CSA approved TWN75, TEW, AWM IA, FT1 constructions. UL recognized for TW, THW, THWN, THHN. Oil resistant I..
100% Modulus 0.0128 - 0.0152 GPa
1.85 - 2.20 ksi
Secant; Conditioned 7 days at RT/50% RH; ASTM D638
AdvanSource Biomaterials ChronoFlex® C 55D Biodurable Medical Grade Polyurethane
ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome..
100% Modulus 0.0128 GPa
1.85 ksi
ASTM D-638
Axiall 16901 Wire & Cable Flexible PVC
90°C rated fiber optic riser jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.